doi: 10.17586/2226-1494-2015-15-2-246-252


BEND-INDUCED LOSSES IN A SINGLE-MODE MICROSTRUCTURED FIBER WITH A LARGE CORE

Y. A. Gatchin, K. V. Dukelskiy, I. B. Bondarenko, A. A. Sadykov, V. V. Demidov, E. V. Ter-Nersesyantz


Read the full article  ';
Article in Russian

For citation: Gatchin Yu.A., Dukel'skii K.V., Bondarenko I.B., Sadykov A.A., Demidov V.V., Ter-Nersesyants E.V. Bend-induced losses in a single-mode microstructured fiber with a large core. Scientific and Technical Journal of Information Technologies, Mechanics and Optics, 2015, vol.15, no. 2, pp. 246–252.

Abstract

A study of bend-induced losses in a silica-based single-mode microstructured fiber with a core diameter ranging from 20 to 35 microns and increased relative air content in the holey cladding has been conducted. With the use of the equivalent step-index profile method in approximation of waveguide parameters of microstructured fiber (normalized frequency and normalized transverse attenuation constant) the effect of bending on the spectral position of the fundamentalmode short-wavelength leakage boundary has been analyzed. Upon measurement of spectral characteristics of attenuation in the considered fibers good accordance of numerical and experimental data has been found out. It is shown that increase of the air content in the holey cladding leads to expansion of the mentioned boundary to lower wavelengths for the value from 150 to 800 nm depending on the core size and bending conditions. A single-transverse-mode propagation is achieved on fiber length of 5-10 meters due to a substantial difference in losses of fundamental and higher-order guided modes attained by bending. Optical losses in all studied samples are less than 10 dB/km at the wavelength λ = 1550 nm. The results of the study can be applied in the design of high-power laser systems having such basic requirements as a relatively large mode spot and high beam quality.


Keywords: microstructured fiber, single-mode regime, large core, optical losses, bend-induced losses

References
1. Tunnermann A., Schreiber T., Roser F., Liem A., Hofer S., Zellmer H., Nolte S., Limpert J. The renaissance and bright future of fibre lasers. Journal of Physics B: Atomic, Molecular and Optical Physics, 2005, vol. 38, no. 9, pp. S681–S693. doi: 10.1088/0953-4075/38/9/016
2. Taverner D., Richardson D.J., Dong L., Caplen J.E., Williams K., Penty R.V. 158-μJ pulses from a singletransverse- mode, large-mode-area erbium-doped fiber amplifier. Optics Letters, 1997, vol. 22, no. 6, pp. 378–380.
3. Baggett J.C., Monro T.M., Furusawa K., Richardson D.J. Comparative study of large-mode holey and conventional fibers. Optics Letters, 2001, vol. 26, no. 14, pp. 1045–1047.
4. Russell P.St.J. Photonic-crystal fibers. Journal of Lightwave Technology, 2006, vol. 24, no. 12, pp. 4729– 4749. doi: 10.1109/JLT.2006.885258
5. Birks T.A., Knight J.C., Russell P.St.J. Endlessly single-mode photonic crystal fiber. Optics Letters, 1997, vol. 22, no. 13, pp. 961–963.
6. Broeng J., Mogilevtsev D., Barkou S.E., Bjarklev A. Photonic crystal fibers: a new class of optical waveguides. Optical Fiber Technology, 1999, vol. 5, no. 13, pp. 305–330. doi: 10.1006/ofte.1998.0279
7. Mortensen N.A. Effective area of photonic crystal fibers. Optics Express, 2002, vol. 10, no. 7, pp. 341–348.
8. Mortensen N.A., Nielsen M.D., Folkenberg J.R., Petersson A., Simonsen H.R. Improved large-mode-area endlessly single-mode photonic crystal fibers. Optics Letters, 2003, vol. 28, no. 6, pp. 393–395.
9. Nielsen M.D., Mortensen N.A., Albertsen M., Folkenberg J.R., Bjarklev A., Bonacinni D. Predicting macrobending loss for large-mode area photonic crystal fibers. Optics Express, 2004, vol. 12, no. 8, pp.
1775–1779. doi: 10.1364/OPEX.12.001775
10. Agruzov P.M., Kozlov A.S., Petrov M.P., Dukel'skii K.V., Komarov A.V., Ter-Nersesyants E.V., Khokhlov A.V., Shevandin V.S. Mode composition of holey fibers with a large seven-element core. Journal of Optical Technology (A Translation of Opticheskii Zhurnal), 2008, vol. 75, no. 11, pp. 747–749.
11. Agruzov P.M., Dukel'skii K.V., Komarov A.V., Ter-Nersesyants E.V., Khokhlov A.V., Shevandin V.S. Developing microstructured lightguides with a large core, and an investigation of their optical properties. Journal of Optical Technology (A Translation of Opticheskii Zhurnal), 2010, vol. 77, no. 1, pp. 59–62.
12. Demidov V.V., Dukel'skii K.V., Shevandin V.S. Modal composition of radiation in microstructured lightguides with a displaced core. Journal of Optical Technology (A Translation of Opticheskii Zhurnal),
2010, vol. 77, no. 6, pp. 394–398.
13. Demidov V.V., Dukel'skii K.V., Ter-Nersesyants E.V., Shevandin V.S. Microstructured single-mode lightguides based on the phenomenon of differential mode damping. Journal of Optical Technology (A
Translation of Opticheskii Zhurnal), 2012, vol. 79, no. 1, pp. 36–40. doi: 10.1364/JOT.79.000036
14. Sakai J., Kimura T. Bending loss of propagation modes in arbitrary-index profile optical fibers. Applied Optics, 1978, vol. 17, no. 10, pp. 1499–1506.
15. Sakai J. Simplified bending loss formula for single-mode optical fibers. Applied Optics, 1979, vol. 18, no. 7, pp. 951–952.
16. Saitoh K., Koshiba M. Empirical relations for simple design of photonic crystal fibers. Optics Express, 2005, vol. 13, no. 1, pp. 267–274. doi: 10.1364/OPEX.13.000267
17. Dukel'skii K.V., Kondrat'ev Yu.N., Khokhlov A.V., Shevandin V.S., Zheltikov A.M., Konorov S.O., Serebryannikov E.E., Sidorov-Biryukov D.A., Fedotov A.B., Semenov S.L. Microstructured lightguides with
a quartz core for obtaining a spectral supercontinuum in the femtosecond range. Journal of Optical Technology (A Translation of Opticheskii Zhurnal), 2005, vol. 72, no. 7, pp. 548–550.
18. Demidov V.V., Dukel'skii K.V., Ter-Nersesyants E.V., Shevandin V.S. Investigation of the single-mode operating regime of microstructured lightguides with radiation-leakage channels. Journal of Optical Technology (A Translation of Opticheskii Zhurnal), 2013, vol. 80, no. 5, pp. 309–312. doi: 10.1364/JOT.80.000309
19. Berenger J.-P. A perfectly matched layer for the absorption of electromagnetic waves. Journal of Computational Physics, 1994, vol. 114, no. 2, pp. 185–200. doi: 10.1006/jcph.1994.1159
20. Agruzov P.M., Dukel'skii K.V., Il'ichev I.V., Kozlov A.S., Shamrai A.V., Shevandin V.S. Guidance properties of few-mode large-mode-area microstructured fibres. Quantum Electronics, 2010, vol. 40, no. 3, pp. 254–258. doi: 10.1070/QE2010v040n03ABEH014230
21. Mortensen N.A., Folkenberg J.R. Low-loss criterion and effective area considerations for photonic crystal fibres. Journal of Optics A: Pure and Applied Optics, 2003, vol. 5, no. 3, pp. 163–167. doi: 10.1088/1464-4258/5/3/303


Creative Commons License

This work is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License
Copyright 2001-2026 ©
Scientific and Technical Journal
of Information Technologies, Mechanics and Optics.

Яндекс.Метрика